Skip to content
فارسیالعربيةDatasheet on WhatsApp
  1. Home
  2. Guides
  3. Granule moisture and drying

Granule moisture and drying

Damp granule is one of the commonest causes of defective parts, and it is not always visible: the pellets look dry, but absorbed moisture turns to steam in the hot machine and ends up on the part.

Which granules absorb moisture?

PolymerMoisture uptakeDrying before production
Polyamide (PA)HighRequired
Polycarbonate (PC)Moderate, but with a bad effectRequired
PETModerate, sensitiveRequired
ABSModerateUsually required
PS, PP and PEVery lowUsually not needed; only surface moisture from condensation or a damp store

What defects does moisture cause?

General drying guidance

The exact temperature and time of a grade come from its datasheet or the supplier; the general range commonly used with a desiccant (dry-air) dryer is: PA about 80 °C for several hours · ABS about 80 °C for several hours · PC about 120 °C for several hours · PET about 160 °C for several hours. An ordinary hot-air dryer is not enough for sensitive materials, and the dew point of the air matters.

A few practical tips

Questions

Must PP be dried?

Usually not, because its moisture uptake is very low; only if the pellets have sweated or sat in a damp store.

Is a silver streak always moisture?

It is the commonest cause, but a very high melt temperature, injection speed and contamination can also cause it; check moisture first.

Where do I see Epic PC and PA?

See the polymer types; the drying instruction comes from the datasheet of each grade.

For a datasheet or sample contact Epic Polymer: +98 919 212 4919 · WhatsApp.

Let's review your part together

Send the part specification or the grade you need; our sales specialist will arrange the datasheet and a sample. Price: on request.

Phone & WhatsApp
0919 21 24 919
Factory address
Tehran, Golestan Town, Baharieh Industrial Estate, Kaj 2, No. 19
CallWhatsApp